Aka-Poly+ 15 µm 1 l

44148015

High Concentration Polycrystalline Diamond Suspension for metallographic specimen preparation.

100% Poly crystalline diamonds
Median (50%) 15.0 µm.
Tolerance 14.2 - 15.8 µm
Upper limit (99%) 21,5 µm


Concentration 40 ct/l

Keep out of direct sunlight.

Click here for SDS/PDS.