Aka-Mono+ 9 µm 1 l

44137015

High Concentration Monocrystalline Diamond Suspension for metallographic specimen preparation.

100% Mono crystalline diamonds
Median (50%) 9.6 µm
Tolerance 9.12 - 10.08 µm
Upper limit (99%) 12.9 µm


Concentration 40 ct/l