High Concentration Monocrystalline Diamond Suspension for metallographic specimen preparation.

100% Mono crystalline diamonds
Median (50%) 5.7 µm.
Tolerance 5.42 - 5.98 µm
Upper limit (99%) 7.9 µm


Concentration 40 ct/l