Quick preparation
DiaDoublo is formulated on the basis of our lubricants Aka-Lube, ensuring a high removal rate and perfect scratch pattern, right from the start. But there are other factors that also matters.
Narrow particle size distribution
When using the hardest wearing abrasives like diamonds, it is important that particle size distribution has the narrowest deviation possible. Large particles will result in deep scratches and require longer preparation times in the subsequent step, and small particles will not provide the required material removal rate, thereby prolonging the ongoing preparation step. We therefore use the most stringently graded diamond particles commercially available.
Modern sorting technology, combined with electronic and optical quality control, ensures highly reproducible preparation results. See our close tolerance at specifications
High diamond concentration
Polycrystalline DiaDoublo has a concentration of 6.7 ct/l, equivalent to a mixing ratio between suspension and lubricant of 1:2. This ensures a combination of high removal rate and perfect scratch pattern.
Monocrystalline DiaDoublo has a concentration of 5 ct/l, equivalent to a mixing ratio between suspension and lubricant of 1:3, for good economic preparation.
On to environment